High gold content ceramic bonding alloy acc. to EN ISO 9693-1 and 22674, yellow

BENEFITS:

  • Gold content 88.7 mass % (precious-metal content 98.4 mass%
  • Universal indication range, suitable for large bridges with more than two units upon installation of special framework strengthening.
  • Suitable for milling
  • Palladium and copper free
  • Contains only gold, platinum, and essential trace elements
  • Excellent corrosion resistance

 

SPECIFICATIONS:

Ceramic bonding alloy acc. to EN ISO 9693 EN ISO 22674
Type 4 (s/ v/ k)
Shade Yellow
Indication 3,4,5,15A)
Composition Au 88.7
Pt 9.49
Zn 1.5
Ir x
Mn 0.1/ Rh 0.2

Technical specifications, melting and casting
Melting range 1055 ° – 1130 ° C
Preheating temperature 850 ° C
Casting temperature 1280 ° C
Crucible Graphite
Density 19.0 g/cm3
Hardness (HV5) 215 (w/k), 220 (v), 180 (s)
0.2 % yield strength (MPa) 520 (w/k), 540 (v)
Elongation (%) 6 (w/k), 5 (v)
Young’s modulus of elasticity (GPa) 90

Ceramic firing
CTE 14.5
Oxide firing 880° C/ 10 min. (vacuum, stripping)
Soft annealing
Hardening 450° C/ 15 min.

Solder/laser welding wire
Solder Herador PF solder 1040, 1010
Herador/Maingold PF solder 800
Laser welding wires Ø 0.5 mm x 200 mm + Ø 0.3 mm x 200 mm

SPECIFICATION LEGEND

Explanation of abbreviations and numbering:

x = content < 0.1 mass%

Indications:

1 Inlays, cervical filling
2 MOD Inlays
3 Crowns
4 Bridges
5 Milling technique
6 Partial dentures
10 Cast posts
14 Can be veneered with high expansion, low-fusing ceramics
15 Implant restorations
16 Electroformed double crown technique (primary crowns)

Abbreviations:

w = after soft annealing and quenching
k = ceramic bonding alloy: condition after ceramic firing
v = after hardening
s = self-hardening after slow cooling in the mould

A = A stable framework design with reinforced connections with a cross section of 8 – 10 mm² is required for long span bridges and superstructures. Additionally, the frameworks need to be hardened.
B = Depending on the copper content, in some cases discolouration ofdouble crowns may result after short period of wearing. Discolouration, however, is technically and physiologically harmless.
C = In exceptional cases these alloys can also be used for traditional telescopic crowns with parallel walls and for the bar casting technique provided that cross-sections for crown walls, approximal areas, bars and laser welded joints are particularly thick and the alloy is hardened subsequently. No indication for conical crowns and sheardistributors.

 

Bio Herador® SG – for C& B
Select the fields to be shown. Others will be hidden. Drag and drop to rearrange the order.
  • Image
  • SKU
  • Rating
  • Price
  • Stock
  • Availability
  • Add to cart
  • Description
  • Content
  • Weight
  • Dimensions
  • Additional information
Click outside to hide the comparison bar
Compare